■ Overview
Hot rolled shipbuilding steel materials ABS Grade DH36,ABS DH36 steel plate,AB D36 ship plate is a higher steel grade among shipbuilding steel.As for the heat treatment for ABS Grade DH36,if the thickness above 12.5mm,the delivery condition must be Normalized or Normalized rolled or TMCP.As rolled is not allowed to delivery without the customer's special requirement.Heat treatment mark would be appear on our each steel plate as steel mark,such as Normalized would be marked as N,TMCP would be marked as TMCP which is short for Thermo-Mechanical Control Process.
■ Full Data
Technical Requirements & Additional Services for ABS DH36 steel plate:
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
♦ High tension test
♦ Z-Test (Z15,Z25,Z35)
♦ Low temperature impacting test
♦ Ultrasonic test under ASTM A435,A577,A578
♦ Cetificated by ABS,LR,GL,BV,DNV,KR,NK,CCS,RINA
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
■ Techicals
►Mechnical property for ABS Grade DH36 shipbuilding plate:
Yield strength (≥Mpa) | Tensile strength (Mpa) | Elongation in ≥,% | |
355 | 490-620 | 200mm | 50mm |
19 | 22 |
►Chemical composition for ABS Grade DH36 ship plate (Heat Analysis Max%)
Main chemical elements composition of ABS Grade DH36 | ||||||
C | Si | Mn | P | S | Al (acid) min. | Nb |
0.18 | 0.10-0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02-0.05 |
V | Ti | Cu | Cr | Ni | Mo | |
0.05-0.10 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |