♦ Eddy current examination using Mafnetic saturation for pipes comply to E309 standard
♦ General requirements for alloy and stainless steel pipes under A999/A999M specification
♦ Heat treatment under normalize and temper with cooling media air or accelerated cooling
♦ Mill test certificate with EN 10204 TYPE 3.1 OR 3.2 with ABS,LR,BV,SGS,TUV,CCS
♦ Packages with wooden cases,woven bags,plastic water-proof bags
►Mechnical property for A335 Grade P911 steel pipe:
A335 Gr P911 steel pipe | |
Yield strength (≥Mpa) |
440 |
Tensile strength (≥Mpa) |
620 |
►Chemical composition for A335 Grade P911 seamless steel pipe (Heat Analysis Max%)
Main chemical elements composition of A335 Grade P911 |
|||||||
C |
Mn |
P |
S |
Si |
Ni |
Cr |
Mo |
0.09-0.13 |
0.30-0.60 |
0.020 |
0.010 |
0.10-0.50 |
0.40 |
8.5-9.5 |
0.9-1.1 |
V |
Cb | N | Al | W | B | Zr | Ti |
0.18-0.25 |
0.06-0.10 |
0.04-0.09 |
0.02 |
0.9-1.1 |
0.0003-0.006 | 0.01 | 0.01 |